A trace drawn with the conductive ink will combine with solder, provided the soldering temperature does not exceed 350°F (177°C) and the solder joint is formed within 5 seconds. If the drawn trace must be soldered to, we recommended that tin/lead solder containing 2% silver be used and that the trace is heat-cured at 150°F (66°C) for five minutes to produce the most durable trace possible.